Pl. furnish details as a minimum .
1)Which corrosion test ?
2)Welding process?
3)What brand of consumables ?
4)Heat input while welding?
5)Which DSS steel - 32205 ?
Pl. send in detail information then the correction/suggestion can be given 

Thanks and regards

Vishwas -IWE


On Thursday, March 9, 2023 at 2:39:40 PM UTC+5:30 mohammed hashif pattambi wrote:
Gents,

during PQR for WPS of SS to DSS using filler Er Ni Cr MO-10, Corrosion test is failing. can i get any advise and suggestion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8eea763e-6489-43b7-9324-aa7483e4b159n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...