Sujit,

Pl. screen through  ASME SEC II C  -  SFA 5.01 Filler metal procurement guidelines.

It enlists various terms related to consumables and its detailed description 

Thanks 
Vishwas - IWE 

 

On Wednesday, February 22, 2023 at 1:18:14 PM UTC+5:30 sujit kumar wrote:
Dear Experts,

What is the requirement of C5 for covered electrodes and the S3 requirement for Bare electrode?




Best regards 
S.K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6eb9c632-6668-4910-983e-78649c9d23e3n%40googlegroups.com.

No comments:

[MW:35693] egwuanimkwujacobisrael@gmail.com

Dear all, No. MPI can only detect defect that is 1 to 2 mm dept. Therefore the paint must have mask the defect. Thanks. Egwuanimkw...