Monday, February 28, 2022

Re: [MW:32942] ER309L DMW

if i use 309, what is the consequences on metallurgical properties.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Feb 23, 2022 at 9:29 AM fikril shaharudin <ahmadfikrilkhairi@gmail.com> wrote:
what should we use if the service temperature greater than 300 degree C?


On Sat, Feb 19, 2022 at 10:51 PM pradip kumar Sil <pradipsil@gmail.com> wrote:
you can use it if the service temp is not greater than 300-degree centigrade

On Sat, Feb 19, 2022 at 7:51 PM pradip kumar Sil <pradipsil@gmail.com> wrote:
Yes, you can

On Sat, Feb 19, 2022 at 7:31 PM Tajuddin Mohammed <tajuddinjntu@gmail.com> wrote:
Dear experts,
      Please kindly clarify if we can use ER309L filler wire for dissimilar welding between P1(A106 Gr B) to P8 (A182 F316L) in gas service
 Your valuable suggestion is highly appreciated.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACZrEUZKfqUesgcm5Z-z8ig%3Dr6KHRedXZk4%2Bg5X9v98vqxf7ZA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kZmykODcV0oc6QYk7vxX4zhDi4%2Bw%2BPdk85uurDoO7pVQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAt_OXzDUhpke%3DLVOkb0HpzorDC6CJ4yzfid2HbMGJ1V36hndw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOpF2Zw6_p8Vwpk%2BKwhksYLaAmCszA%3DqzmJhargSY8S9g%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...