Wednesday, February 23, 2022

Re: [MW:32917] CS to Inconel 625 Material _ Suitable Welding Consumable

ERNiCrMo-3 or ERNiCrMo-10



Inline image
Inline image


Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 23 February, 2022, 08:07:20 am GMT+4, Manikandan J <mechmani22@gmail.com> wrote:


Dear All,

What is the Suitable Consumable for CS to Inconel 625 Material for GTAW & SMAW Material.

Process : GTAW & SMAW

Regards,
Manikandan



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNk3ySUGffFw_3pVtosNQj_4AS3S-w9HKS4Bud54qEbDQ%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...