ferritic steels can be hardned 
Στις Τετ 16 Φεβ 2022 στις 9:30 π.μ., ο/η Kannayeram Gnanapandithan <kgpandithan@gmail.com> έγραψε:
Less Carbon, High Chrom and some small addition of alloying elements Nb, Ni etcU can not hardened by heattreatmentTHANKS & BEST REGARDS,KG.PANDITHAN, BE, IWE, CSWIP 3.1,ISO 9712 Level 2 in VT,ASNT-Level II in PT,MT,RT & UT,LA ISO 9001-2015,International Welding Engineer.CONSULTANT-WELDING & QUALITYMobile no: +919940739349--On Wed, Feb 16, 2022 at 8:52 AM SN <suryawanshinileshj@gmail.com> wrote:Dear all,--What is the exact defination of ferritic steel as per ASME or ASTM or EN standard.Kindly clarifyRegards
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7M_Yv5pZ2eRgWjLGTcXPwtBRTM0S5o1idRkeMAmidU-TA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNDwXmnAYhfszjsxCU-GPvQZMk%3DtnDcTj2BGehpPK7v_w%40mail.gmail.com.
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BdCtwdjXB8NfFtPxMUzx7Su%2BaeMZ1mEw4RfdDw7EQvBQ%40mail.gmail.com.
Comments