Thursday, February 17, 2022

Re: [MW:32892] Procedure for PQR preparation

Prepare PWPS as per requirement.

On Thu, Feb 17, 2022 at 1:47 PM Shahil Saini <sainishahil98@gmail.com> wrote:
Hello everyone,
Hope you are doing well,

From where to begin the preparation for PQR?
Should I first produce a production test coupon and enter the exact details used at the time of test coupon preparation.

Kindly advise further,

Regards,
Shahil Saini

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__XoSPYoPp5_hQyJWMaXKSM4xKJN1mcOqaEm6oKeNG0gw%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RNPjj4X6w2qrhB74%2BMLY3G%3DvVewgfD8ghDS9eo2HaN-cg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...