RE: [MW:32881] Ferritic Steel

All Carbon &  Low Alloy Steels are Ferritic Steels. They can harden subject to the heat treatment and cooling rate. However, the term "Hardening" does not apply for BPV equipment & piping as the steels used for these components are fairly low carbon and well manufactured with a lot of quality norms. Hardening is more pronounced for steels with higher C Content, typically > 0.30 %.

 

Ferritic Stainless steels are not amenable to hardening following heat treatment. They only can be annealed. Read these  articles for general  introduction: 3.7.2 Heat Treating Stainless Steel | Forging Industry Association.

An overview of austenitic and ferritic stainless steels (thefabricator.com).

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Jenish Mistry
Sent: February 16, 2022 5:35 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:32875] Ferritic Steel

 

Dear sir,

 

Why it cannot hardened by heat treatment?

 

By which process it can hardened ??

 

 

On Wed, Feb 16, 2022 at 1:00 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:

Less Carbon, High Chrome and some small  addition of alloying elements Nb, Ni etc.

U cannot hardened by heat treatment


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  CSWIP 3.1,

ISO 9712 Level 2 in VT,

ASNT-Level II in PT,MT,RT & UT,

LA ISO 9001-2015,

International Welding Engineer. 

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

 

On Wed, Feb 16, 2022 at 8:52 AM SN <suryawanshinileshj@gmail.com> wrote:

Dear all,

 

What is the exact definition of ferritic steel as per ASME or ASTM or EN standard.

 

Kindly clarify

 

Regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7M_Yv5pZ2eRgWjLGTcXPwtBRTM0S5o1idRkeMAmidU-TA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNDwXmnAYhfszjsxCU-GPvQZMk%3DtnDcTj2BGehpPK7v_w%40mail.gmail.com.


 

--

Thanks for your best support.

 

Regards,

Jenish Mistry

09033476117

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_cDKpB79gZWrMbOqCsWxznU1-47GDPmj8cC5cKpXcdXMQ%40mail.gmail.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...