Monday, February 14, 2022

Re: [MW:32862] nominal thickness

Check uw-40


On Mon, 14 Feb 2022 at 7:33 am, 'Prakash Hegde' via Materials & Welding
<materials-welding@googlegroups.com> wrote:
Hi
Nominal the is to be considered as weld metal the for deciding Pwht soak time
Regards
Hegde


On Mon, 14 Feb 2022 at 8:47, m zareei
<zareei.int@gmail.com> wrote:
What is the nominal thickness (for using in ucs-56) when two parts connected together are the same as in the following figure? Please answer with its standard reference.
image.png
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANBpwvXnitxStVHzpMmrKbRD7cXznfNbX_X%2B%2Bp5zj5mjAjJsWw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1081246884.886066.1644809488391%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/866479614.768468.1644814744646%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...