Re: [MW:32831] REQUIRED FILLER WIRE FOR (ASTM A312-Gr UNS 31254) Super Austenetic Stainless Steel

Hello Everyone,

Why filler wire selection of A 312 UNS 31254 is not mentioned in Table 6 of SA 312 of ASME Sec II Part A1? 



On Tue, Feb 8, 2022 at 8:47 AM Muhammad Azeem <azeem7999@gmail.com> wrote:
Gents,
I need your valuable support to assist about the filler wire to be used for Super Austenitic Stainless Steel (ASTM A 312 Gr UNS 31254) ??




Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yAQ5mG4ZSP1b8dm-3X7HWASTFGeuv0Y_s2hqR-qGHH2mw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-d-0ndkOGabk%3DtJ1Y6Qi6CoBObO9WG8cc5oY3TFRL1%2Bw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...