Re: [MW:32819] Re: 98%Ar+2%O2 or 98%Ar+2%CO2

o2 is better than co2 for ass, but either one can be used.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Feb 5, 2022 at 5:43 PM Mohd Siraj <mohd52100@gmail.com> wrote:
depend on the mode of transfer,

for Gas details pl refer SFA 5.32 for details instead of random selection.

On Friday, February 4, 2022 at 11:26:18 AM UTC+3 S.Sankalp wrote:
Dear All,

Please comment on the weld metal properties of GMAW welded ASS with shielding gases 98%Ar+2%O2 and 98%Ar+2%CO2. How a shielding gas among these two will be selected.

Regards,
Sankalp

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/267a35fa-fa09-4d65-9293-8ca653e2cc30n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMTPR3w7pUHC_suBsVoxcnXwGJiXMjhU%3DsF7Rkr3vkT2Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...