[MW:32896] FW: 32891] RE: 32887] Qualification of WPS for DSS

 

Hi,

 

Your query does not specify the intended service? However, application of Duplex Stainless steels in pipelines are typically for offshore O&G carrying and processing pipelines. DNV guidelines are followed a lot for such design conditions. You may take a look at this attached specification and read through some of the highlighted guidelines. Usually for such pipelines involving Duplex Stainless Steels many of the technical requirements are client driven. If your project has specific requirements those would be more binding that the attached specification.

 

 

Thanks.

 

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf of Benaouda Mezrar

Sent: February 17, 2022 5:15 AM

To: Materials & Welding <materials-welding@googlegroups.com>

Subject: [MW:32887] Qualification of WPS for DSS

 

 

Hi expert

 

In which code I can find the essential variable for qualification of the WPS for DSS pipeline thanks for your help friend and have good day

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com <https://groups.google.com/d/msgid/materials-welding/1a4d5a1a-9635-42b4-a2d5-acb0b900097dn%40googlegroups.com?utm_medium=email&utm_source=footer> .

 

 

 

________________________________

 

<https://www.avg.com/internet-security>   This email has been checked for viruses by AVG antivirus software.

www.avg.com <https://www.avg.com/internet-security

 

 

 

 

--

https://materials-welding.blogspot.com/

https://www.linkedin.com/groups/122787

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com <mailto:materials-welding+unsubscribe@googlegroups.com> .

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com <https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAADWLpon/diTQqsz0R8H27cbAQAAAAA%3D%40rogers.com?utm_medium=email&utm_source=footer> .

 




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...