Thursday, February 17, 2022

[MW:32887] Procedure need for reinforcing pad

Dear all

         I have one Doubt regarding the reinforcement pad which is designed by B31.3. I get all the clearances from the design team. But I just wonder if the pad will be cut by two pieces lateral to run pipe and merged on the location. 

          My Client told me that the case is code wise ok. 

          So now I have to Submit my WMS for that work.

          In B31.3 there is nothing about it. So please generals if you have any about that ... Please share with me.

Herewith I attached the Photo also




--


==============
Thanks & Regards

SUNGDO ENGINEERING 
MARUTHU PANDIAN.N
Engineer (Piping & Quality Control)
Polimery Police PDH/PP Project, Poland
Mob +48571461164

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ3bEeXbpLZnKVLYEwH0NpKkP6Het6i6raC2EwEHSBYg_049Kg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...