I have an existing WPS-PQR of SMAW process with impact testing requirement. Since the PQR was done with a 38mm plate the base metal thickness qualified is from 16 to 200mm when impact testing is required. For the same job where I have to do Tack welds for the fit-ups will this WPS-PQR suffice for the tack welds? or a separate WPS-PQR will be required?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/067a69af-f523-4817-86ae-7c92239d9b62n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...