[MW:32813] Re: PWHT soaking time for impact testing applicable vessel

yes, acceptable, there is ASME interpretation.

I try to attach it but was not able to attach it.

On Wednesday, December 8, 2021 at 9:20:51 AM UTC+3 ibratech wrote:
Gentle men,

A pressure vessel required PWHT, and Impact test. The vessel thickness is 46 mm. The PWHT of this vessel required as per code is 108.6 minute.

The contractor submitted a PQR which is performed 60 minutes (1hr)  and  720 minute (12hrs) PWHT and and all mechanical test done in both holding time.

As ASME sec IX, clause 407.2 

"
QW-407.2 A change in the postweld heat treatment
(see QW-407.1) temperature and time range
The procedure qualification test shall be subjected to
PWHT essentially equivalent to that encountered in the
fabrication of production welds, including at least 80%
of the aggregate times at temperature(s). "

As per the above clause the PQR is acceptable?. It does not meant PQR shall be essentially equivalent within 80% of actual production PWHT?. Since the manufacture done 60 minutes and 720 minutes, and the production PWHT comes in between holding time (108.6) the PQR will be acceptable?

 
Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b875b18c-50f5-4da3-83c8-c8d8c450a19dn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...