Hello Guys,
Below image extracted from cswip 3.1 book, for your reference:
Syed Gohar Abbas Zaidi
-- 
On Tue, Jan 25, 2022 at 8:27 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
--I suppose BARC regulation is mostly related to Radiation Safety & ASME code for the technique & procedures. Some Client specification covers this requirement or you need to get it from Radiography company or source supplier.Please check the below Link for some details.Thanks & Regards
J.Gerald Jayakumar
On Tuesday, 25 January, 2022, 08:51:25 am GMT+4, Jenish Mistry <jenishmistry1992@gmail.com> wrote:Hi Rishikesh,Can you please share a snap for where it is mentioned in ASME or BARC for my reference.if possible can you please share BARC regutary for Radiography Source for my reference ????On Mon, Jan 24, 2022 at 3:17 PM rishikesh shahi <rishikeshshahi@gmail.com> wrote:60mm with IR192... There after we have to carry out the RT by Cobalt 60.....Regards..Rishikesh ShahiHOD QA/QCM/S FABTECH ENGINEERING PVT. LTD. NAGPUR, MAHARASHTRA--On Mon, 24 Jan 2022, 3:06 pm Manish Kumar, <mkmkr431@gmail.com> wrote:Dear Sir,--As per which, ASME clause or BARC regulatory, How much thickness of radiography can be carried out from Iridium 192 source.--RegardsManish KumarInspection(Mechanical) EngineerPDIL-HURL Barauni site
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k5eBcnvrHW-eO86oNUsxgc19YoViaTT3U9TfMSjMzu1HQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFf3VQNNRMPYzgaee-Fv_jC_1QUP7W9i7Bm9uN-xp6DD9J%2BXXw%40mail.gmail.com.
----Thanks for your best support.Regards,Jenish Mistry09033476117
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_e6k-oO489uvtHm%3Dgmv2XaVmHzpN0MSUk9CfDpQJi5LRA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1063941795.1032724.1643087828977%40mail.yahoo.com.
Regard's:
Syed Gohar Abbas Zaidi
Cell No.: 0092-324-1407544
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGOPWRvvzYqQXu8PKoPVxL420w_txAXrTnYor_kVkw5-GONDjA%40mail.gmail.com.
Comments