Re: [MW:32759] impact test difference in WPS & MTC

Consumable should have tested for minus 52,  otherwise it may vary
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Jan 17, 2022 at 3:02 PM 'sangram routray' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Experts,
we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact value @ -40°C.

Job's Impact requirement is -52°C.

shall I use the same specific batch Filler wire for the job?? (Y/N)
or required batch test qualification (all weld test )
Answer with code's justification.

 welding code ASME Sec-IX

code of construction ASME B31.3

Thanks & Regards

Sangramkeshari Routaray


MOB NO. +91-8249921885

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/215105493.712317.1642408446087%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN--%3DHhhm-Cv6tmE-vaGVBMbWJnqeSk%3DbKj2HRMyEsZiQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...