Re: [MW:32748] SS 316 clad thickness measurement

You can choose Olympus 45MG equipment.
It will measure both base metal and clad thickness.

Best Regards 
Neilashkumar P 


On Wed, Jan 12, 2022 at 12:09 PM, Chintan Raval
<chintan51@gmail.com> wrote:
Dear Expert

Kindly advice,

For CRO application of ss316L cladding using various welding process such as esw smaw fcaw saw etc for measurement of clad thickness which instrument is suitable.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS40%3D8hyGc6o%3D-6DO%2BiqYUwfwiYHjtbPnibT9PyE5oLgHbA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/802350282.1726023.1641970495351%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...