Friday, January 7, 2022

RE: [MW:32737] Requalification of consumable after shelf life

Hi ,

Every welding consumable has a "shelf life". Please see the guidance from ESAB on typical shelf life of various SMAW electrodes & other FCAW products. Shelf life matters a lot , on how the consumables are manufactured and subsequently stored.

Sec-IX , would not provide any guidance on welding consumables.

If needed all weld metal testing may be performed as per ASME Sec-II, Part C.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

IndependentWelding & Metallurgical Engineering Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of MW
Sent: January 7, 2022 3:14 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:32736] Requalification of consumable after shelf life

 

pl. refer old posts in the group

 

On Friday, 7 January 2022 at 13:38:44 UTC+5:30 Syed Gohar Abbas Zaidi wrote:

Dear,

 

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

 

On Thu, Jan 6, 2022 at 12:10 PM SN <suryawans...@gmail.com> wrote:

Dear all,

 

Can we requalify welding consumables (electrode and wires) once the shelf life is over?

 

As ASME code gives any guideline to requalify the welding consumables.

 

Kindly provide your expert opinion on this.

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


 

--

 

 

 

Regard's:

 

Syed Gohar Abbas Zaidi

Cell No.: 0092-324-1407544

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eacf84d4-13c3-4189-96ba-e117cc1072e5n%40googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...