Normally we do not use welding consumables beyond the Shelf life as recommended by welding consumable manufacturer. I have physically seen Flux coating peeling off from the electrode. It is better to contact the welding consumable manufacturer and if they recommend better to do consumable testing as per ASME Sec.IIC at the manufacturer's premises.

Thanks & Regards

J.Gerald Jayakumar




On Friday, 7 January, 2022, 12:08:41 pm GMT+4, Syed Gohar Abbas Zaidi <gohar.qaqc@gmail.com> wrote:


Dear,

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

On Thu, Jan 6, 2022 at 12:10 PM SN <suryawanshinileshj@gmail.com> wrote:
Dear all,

Can we requalify  welding consumables (electrode and wires) once the shelf life is over.

As ASME code gives any guideline to requalify  the welding consumables.

Kindly provide your expert opinion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


--



Regard's:

Syed Gohar Abbas Zaidi
Cell No.: 0092-324-1407544

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGOPWRvqgUthDZ8UL7vfdNbVTsaZ9H1RrA2%2BukY7xYndxEDjZQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...