Friday, January 7, 2022

Re: [MW:32736] Requalification of consumable after shelf life

pl. refer old posts in the group
Screenshot 2022-01-07 134237.jpg


On Friday, 7 January 2022 at 13:38:44 UTC+5:30 Syed Gohar Abbas Zaidi wrote:
Dear,

This is not possible and there is no direction on ASME section IX as it is solely part of the manufacturer, once shelf life finishes you can further use those electrodes.

On Thu, Jan 6, 2022 at 12:10 PM SN <suryawans...@gmail.com> wrote:
Dear all,

Can we requalify  welding consumables (electrode and wires) once the shelf life is over.

As ASME code gives any guideline to requalify  the welding consumables.

Kindly provide your expert opinion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7PpU8iBW3_ZOqHZJB6Vjzx0Hb8Kh7WAHexA8YzKYtnAEA%40mail.gmail.com.


--



Regard's:

Syed Gohar Abbas Zaidi
Cell No.: 0092-324-1407544

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eacf84d4-13c3-4189-96ba-e117cc1072e5n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...