Hello everyone,

If 4-5 mm welding is performed in the 32 mm thick material, is PWHT & Hydro required or not or can I skip PWHT and Hydro? any clause related to this??




Regards,
Shahil Saini
PGET-Welding

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9cFtaCVyaygJ4L8gXRqSVXs_L8PYTzOMYKOidgcOYVeQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...