Skip to main content

Re: [MW:32676] Impact test ASME b 31.3 ed. 2020

If Design says...impact test is exempted; then you can use non impact wps pqr.

On Fri, 10 Dec 2021, 14:30 ROLANDO RC, <soldadurasrc@gmail.com> wrote:
hi i agree ..... but if i use the code exceptions using impact certified base materials and consumables cooler than design i can avoid impact testing on my PQR right?
Thank you


El viernes, 10 de diciembre de 2021 a las 0:58:08 UTC-3, mhaskar aly escribió:
Hi
Impact test is supplementary essential variable; you need to qualify WPS for this if impact test is applicable to your Job as per Design.

Once you demonstrated impact properties with any combination of base metal and filler metal on PQR, then in production joints it will be waived.

Only when PTC us applicable as pet Code, you need to do additional tests.

Mhaskar Ali
Dubai 


On Fri, 10 Dec 2021, 07:21 ROLANDO RC, <soldad...@gmail.com> wrote:
Good afternoon, My name is Rolando and I just registered. The forum is excellent!

I bring the following doubt about the table Table 323.2.2 Requirements for low temperature toughness tests for metals ASME B31.3 2020

As we can see, it has a revision in table A-3 (b) (2020) where I understand that if I have a certified welding consumable with impact test I can exempt said test in the WPS qualification, for example:

If I have a SA-333 gr 6 material with manufacturing certificate and charpy according to the standard (18 J to -45), it can be welded with a consumable E 7018-1 certified by the factory with charpy (27 J to -45)
If I use this combination on my PQR, can I waive the impact test on my PQR weld? ... assuming I already have a metal base and a factory crash tested consumables certificate? (then I interpret table 323.2.2 table A-3 does not speak of the ZAC)

greetings and thanks!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3d5a4255-54a6-4577-a541-5fc1201f51c6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4ba22454-69a1-40fb-b5bb-78a4433cf259n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4hjb%3D2f9W7V1JrN1yrwQbfvJsB-i-CRgW1Gb2wdEDB7yA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...