Tuesday, March 30, 2021

Re: [MW:32122] RWC (Responsible Welding Coordinator)

Please refer ISO 3834-5, Annex A. 
I think you can sign the document. 


On Tue, 30 Mar, 2021, 5:00 pm ilkinhasanov, <ilkinhasanov.91@gmail.com> wrote:
Hi Gents,

Could you please advise ; does RWC (ISO 3834-2) can issue/sign WPS & WPQR and is it requirement of Standard/Codes that  RWC should has a IWE Diploma for this?.



Regards,
Ilkin HASANOV

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ae3963c3-d53c-4bfa-a484-e59726641cc7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADNMk%2BKZrPJks6BQcA11vWj6LjvEtDpRJX_SSurm9HqNCNjh5Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...