Re: [MW:32051] S275JR to A36 WPS

No need A36 is equivalent to S275 Some times S235 Depend on its YS so no need to make new WPS 

Regards,
H.A 

On Sat, Mar 6, 2021 at 4:23 PM Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Need separate PQR  as S275 is unassigned material 

On Sat, Mar 6, 2021 at 3:08 PM Vishnu Nandan <nandan.vishnup@gmail.com> wrote:
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51ecf34c-72ac-4780-a050-c0d45b9f41b6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OEJ0mDagpRNQwdp8kDUezz%3DRv6_ir81DoFrnHE%3D92GeQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzdNwMTEXTZYeMMVFqVYBcccPzKpYt4Yjvt6ZJAH%3DAJUsg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...