Re: [MW:32083] REGARDING SAMPLE COPY OF CS PIPE TO SS PIPE WPS & PQR

If you plan to use the welding process GTAW, you can use the filler metal ER309L

Vào Th 5, 18 thg 3, 2021 vào lúc 11:54 Kishor Swaminathan <kishors28@gmail.com> đã viết:
Dear Experts ,

Anyone have WPS AND PQR  for CS Pipe to SS Pipe  

NOTE :  we want to weld:  SA240 GR.316L   to  API 5L GR.B PSL 
           Please check the attached drawing . we want to weld item no. 7 to item no.8


Thanks in advance 

KISHOR 
WELDING INSPECTOR 





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPd%2B2RTU%3DSUt8eJBTt7%2BZLsFAtia%3DYSRTDeBXu9-1sXQFYX2gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OnEpB3-tm2m5_4pO6L2kFdSWbmSTU0Qbm-94ysuKatfUA%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...