Refer ASME SEC IX Table QW-452.3
1. Welder can weld max 11.08 thickness as per your JCC. So cant able to weld 12.7 mm thick job2 The welder can weld minimum dia 2 7/8 inch (73mm) OD to unlimited as per your JCC,So cant able to weld 1 inch OD.
On Sun, Mar 7, 2021 at 11:26 AM Ganesh Muthurajan <qceng.mg@gmail.com> wrote:
Hi gentlemen--I have doughty in welder qualification.The welder having two jcc.1. GTAW - OD - 1inch, Thickness- 11.08mm, P no. 34, F no 342. GTAW+SMAW - OD - 2 7/8 Inch, Thickness - unmimited, P No. 1, F no. 6.Now my doubt isThe welder can weld ?1. CuNi - 12.7 mm thickness2. CS - 1" ODHow? If not why?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmF%2BwEcrFhPnEXJFvizXJo9SePFQLKS1%3D-tBE2c_6Q_h6tw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAERXeWnAXkN69FbBkYV6n30JWx-MqvgJ%2BdWq7tDLdT9yWQUOeA%40mail.gmail.com.
Comments