Saturday, March 27, 2021

[MW:32106] Radiography on Bronze casting material

Dear Experts
Need opinion on radiography source selection for bronze casted raw material sleeve of size  OD 400mm X ID 364mmn X Length-446mm.

Grade CuSn12Ni2-CG (DIN EN 1982)

What are factor need to consider for the radiography testing on this material. What is the sensitivity of the same?



Regards
Suresh


--