Could you please advise, when does ASME B31.3 require to perform Charpy Test for Inconel Material (UNS 06625)?
After which MDT it is mandatory to perform it?
Regard,
Ilkin HASANOV.
-- https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYXdxMbYXHYBV%2BRaKidjv7B%2BB_x7%3Dw8Mz5h1k-Nm%2BfiQg%40mail.gmail.com.
Comments