Friday, March 26, 2021

Re: [MW:32102] Impact energy Vs Structure

What is the difference between BCT and FCT structure?

On Thu, 25 Mar, 2021, 9:29 am Vinoth kanna ramachandran, <srvkanna1@gmail.com> wrote:
Dear sir,

Greetings for the day 

Mild steel - BCC structure (body centred cubic ) 
Austenite stainless steel - FCC structure (face centered cubic) 
Martensite - FCT structure  ( face centred tetragonal )

coarse grain means - less FCT crystals , fine grain means - More FCT crystals. 

Tetragonal structure can't absorb more impact energy , due to its crystal structure , since it prevents its movement . if it's fine grain , still more difficulty to absorb energy . 

That's why FCC crystals have better impact properties than any other in the steel family .Fine Grain FCC - greater impact energy absorption.



Regards

Vinoth kanna
QC- welding & piping inspector 
Manifa Project

API -510, CSWIP 3.1, NDT level II - UT, RT ,PT, MT, VT,LT,Infrared & Thermography 
Technical - Metallurgy

Contact : M - +91-9787954338,+966-539127946
              Email id : srvkanna1@gmail.com


On Thu, Mar 25, 2021 at 8:43 AM EmaD FaRaHanI <emad.farahani@gmail.com> wrote:
Dear Friends,
Consider we have a mild-steel, cooling fast from welding temperature, we must have a fine grain structure with martensite formation.
Hypothetically, considering that we want to use this structure. I was wondering what is the relation between the impact energy and the structure? will it be decreased due to martensite formation? or increased due to fine grain? I understand that we don't use the martensite state of structures and we need to quench and tempering them.

Thanks,
Emad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFboLm6H50x3K8NLgFACWovNv1ETBoBudSrKunaHFm_aw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbO-YZjzSNu3kGJDJAAJYAYHWwX2AbpE0%2BtueJ%2Bkf2y_C9MZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA-uzKUXKpQPHXFCVZjG_FzZDwciJcX71Xja3CjyDgvQcQuZ8g%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...