Re: [MW:32077] SMALL DIAMETER PROCEDURE QUALIFICATION AS PER ASME SEC IX

Diameter is not an essential variable for PQR. Why you torture your self?

Στις Πέμ, 18 Μαρ 2021 στις 5:07 π.μ., ο/η Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> έγραψε:
Dear Experts ,

PQR is to be qualified  for 
6.35 mm OD X 0.89 mm thickness 
Welding Process - Autogenous Fusion - GTAW Orbital WELDING 
Code - ASME SEC IX 
Material - SA 213 TP316L
Tensile test - 2nos 
Face bend test - 2nos
Root bend test - 2nos 
Full section tensile test is carried out and found satisfactory 

Bend test samples can not be prepared due to less thickness(0.89mm) and small diameter (6.35mm).  Pipe Sectioning  as per permitted by ASME  for small diameter is tried  but could not do it .
When tried to  cut into sectioning for  bending test piece preparation , pipe is getting bent and sectioning is not possible .
 Experts , Pl. help how to go about bend testing or any other way forward 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6e39e586-dc33-4c22-a83e-30255b37a887n%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CfzfiwXorbO-v93Uqkk1u2pv7xyBC5d7FUmZ38ECkuew%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...