Dear Friends,
Consider we have a mild-steel, cooling fast from welding temperature, we must have a fine grain structure with martensite formation.
Hypothetically, considering that we want to use this structure. I was wondering what is the relation between the impact energy and the structure? will it be decreased due to martensite formation? or increased due to fine grain? I understand that we don't use the martensite state of structures and we need to quench and tempering them.

Thanks,
Emad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFboLm6H50x3K8NLgFACWovNv1ETBoBudSrKunaHFm_aw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...