Re: [MW:32027] S275JR to A36 WPS

Even though procedure and everything will be same . S275JR is still unlisted in asme so you will need a seperate wps.

Regards

Chris

On Sat, Mar 6, 2021 at 15:08 Vishnu Nandan <nandan.vishnup@gmail.com> wrote:
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51ecf34c-72ac-4780-a050-c0d45b9f41b6n%40googlegroups.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACY3QXR%3DQNSh8p2K6Zc%3D-Hk0aKW95xzo_jj2oYqkV5ixmBRcmw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...