Sunday, March 7, 2021

Re: [MW:32032] Welder qualification

1. CuNi - 12.7 mm thickness  -  Not permitted 
    Reason - 
    F NO  34 - Welder qualified up to 11.08  mm only .
    Maximum metal qualified  is qualified using F NO 6  filler wire  and NOT with F NO 34 

2. CS - 1" OD -  Not permitted
    Reason - 
     Welder qualified  from   OD 73 mm   and above  with F NO 6 .
      So P NO 1  + 1 "  OD  using F NO 6  filler wire is not permitted 

  F NO of one qualification  and   diameter  of other qualifications can not be  considered for production welding.

  


On Sun, Mar 7, 2021 at 11:26 AM Ganesh Muthurajan <qceng.mg@gmail.com> wrote:
Hi gentlemen 

I have doughty in welder qualification. 


The welder having two jcc.

1. GTAW - OD - 1inch, Thickness- 11.08mm, P no. 34, F no 34

2. GTAW+SMAW - OD - 2 7/8 Inch, Thickness - unmimited, P No. 1, F no. 6.


Now my doubt is 

The welder can weld ?

1. CuNi - 12.7 mm thickness 

2. CS - 1" OD

How? If not why?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM0EmF%2BwEcrFhPnEXJFvizXJo9SePFQLKS1%3D-tBE2c_6Q_h6tw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3O4Qb3pWdQyxsMRznnrnLpaeyfDyYHCbijo80WjJcMydw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...