The bigest risk is to get in contact with carbon Steel or copper alloys

Στις Παρ, 18 Δεκ 2020, 06:37 ο χρήστης ilkinhasanov <ilkinhasanov.91@gmail.com> έγραψε:
Hi Gents,

Is there any specific Standard or Guideline , where I can find storage requirements for Stainless Steel materials (Spool and pipes)?

Is there any potential hazards regarding contamination of pipes/spools when they stored in the open air (sometimes under rain-on the wood pallets)??

Regards,
Ilkin Hasanov  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9791e38f-41c9-44b9-ab93-a0ef86f9a584n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C%3D32FkcR%3DyqXEdzXqkhiOARuqLtMonG9DnO8g3%2BfuH-A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...