you cant use 6010 in straight polarity as it is not built for that. 

On Tuesday, 15 December 2020 at 13:17:58 UTC+5:30 dusroni wrote:
Dear All,

Please Clear me, can we use Polarity DCEN for 6010 electrode welding in piping or pipelines.
If used, explain me how?

  
With Regards

Udaya bahaskar.D

--