Re: [MW:31838] Repair WPs

7010 you must be doing downhill and 7018 uphill progression. So your progression will change. 

On Thu, Dec 3, 2020, 3:37 PM Mohan q8 <mohanq8@gmail.com> wrote:
Dear, 

Pls clarify that your construction code is Piping of Pipeline?

For Pipeline and as per API 1104 you need to have qualified Repair WPS for repair. 

On Thu, Dec 3, 2020 at 10:28 AM udaya bhaskar <dusroni@gmail.com> wrote:
Thank you for your advice.
But as per API1104 both F number is A5.5 . 
Table 1—Filler Metal Groups


On Thu, Dec 3, 2020 at 9:33 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
u can not use 7018 in place of 7010  because Fno is different which is an essential variable.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Dec 3, 2020 at 11:28 AM Jamie Reyes <jamiejrmachineco@gmail.com> wrote:
If no impacts are involved, then yes. If I'm understanding you correctly, that is.....

On Wed, Dec 2, 2020 at 7:30 PM udaya bhaskar <dusroni@gmail.com> wrote:
Dear Giants,

I want to know about little doubt on piping welding repair WPS.
WPS made with 6010 and 7010 electrodes for regular welding.
Now I can plan with  6010 and 7018 electrodes for Repair WPS on the same .
Material :API5L PSL2 grade P1G1
is it allowable?
please correct me.
--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM0cJ%3DZOxjEpLzSnLu-ujsbFjpP4pYz71G-D9VXHwwC6A%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUOEpNymfFOt3bU_uc%3DyiLvW8FQhoCx7wFDSCM%2BOH1pcGw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO7HONFXw1%2B0N8EhyTkL-p3Tpje-jXr6v7AHBQ88oF3ow%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RO5oEWD7_Rziv30ay2ja985A7N334%3DRO1UhMM83SmB0yA%40mail.gmail.com.


--
With Regards,

Mohan, Q8.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALg_OCyb1fFH%3DNOgf%3DXDsEV7tH7y1t%2Bht2KJjB25nZV8s51D%3DA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-Turaw2%2B6woZvQHTLrXw0rYnWE_ww1UJZouMsfwJnx6LS3A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...