Re: [MW:31861] 2% Ceriated Tungsten Electrode.

it is better than thoriated in amperage capacity and this will not emit X-rays while sharpening. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Dec 16, 2020 at 9:16 PM tzhn...@gmail.com <tzhng.lim@gmail.com> wrote:
Hi, 

Does anyone know, at what amperages, the oxides will migrate to the heat at the tip of 2% Ceriated Tungsten Electrode? 

Thanks, 
Tim 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/60752a26-eee4-499e-9394-6f25c1fa4ccdn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMBEQeVHj0nrsHt1o%3DKoUSgx2%3D%2BcwEnf6xv6z%2BcQEi01w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...