On Thu, Dec 3, 2020 at 9:33 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
u can not use 7018 in place of 7010 because Fno is different which is an essential variable.THANKS & BEST REGARDS,KG.PANDITHAN, BE, IWE, CSWIP 3.1,ISO 9712 Level 2 in VT,ASNT-Level II in PT,MT,RT & UT,LA ISO 9001-2015,International Welding Engineer.CONSULTANT-WELDING & QUALITYMobile no: +919940739349--On Thu, Dec 3, 2020 at 11:28 AM Jamie Reyes <jamiejrmachineco@gmail.com> wrote:If no impacts are involved, then yes. If I'm understanding you correctly, that is.....--On Wed, Dec 2, 2020 at 7:30 PM udaya bhaskar <dusroni@gmail.com> wrote:Dear Giants,I want to know about little doubt on piping welding repair WPS.WPS made with 6010 and 7010 electrodes for regular welding.Now I can plan with 6010 and 7018 electrodes for Repair WPS on the same .Material :API5L PSL2 grade P1G1is it allowable?please correct me.----With RegardsUdaya bahaskar.D+919676270121
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM0cJ%3DZOxjEpLzSnLu-ujsbFjpP4pYz71G-D9VXHwwC6A%40mail.gmail.com.
--Regards,Jamie ReyesJ.R. Machine Company, Inc.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUOEpNymfFOt3bU_uc%3DyiLvW8FQhoCx7wFDSCM%2BOH1pcGw%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO7HONFXw1%2B0N8EhyTkL-p3Tpje-jXr6v7AHBQ88oF3ow%40mail.gmail.com.
With Regards
Udaya bahaskar.D
+919676270121
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RO5oEWD7_Rziv30ay2ja985A7N334%3DRO1UhMM83SmB0yA%40mail.gmail.com.

Comments