Tuesday, December 15, 2020

Re: [MW:31847] Polarity

DCEP 

Good Penetrative 

Regards, S.SENTHILKUMAR


On Tuesday, 15 December, 2020, 01:17:54 pm IST, udaya bhaskar <dusroni@gmail.com> wrote:


Dear All,

Please Clear me, can we use Polarity DCEN for 6010 electrode welding in piping or pipelines.
If used, explain me how?

  
With Regards

Udaya bahaskar.D