Dear expert, 

I have B91 material to be weld, 6mm and 10mm thickness, however project requirement need to test -20degC impact which I don't really agree due to Cr-Mo is not intended for low temperature application. 

I performed PWHT 770degC x 1hr but unable to achieve desired charpy, I was wondering if I extend holding time for 6hr, is it possible to achieve -20degC? (Average 40J). 

Welding Process: SMAW and GTAW 

Could anyone advise and guide how to achieve desired impact ? 

Best regards,
Pravin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7e%2B2Vea_Vc61p4Gnfm4Yp%3DU3SasP_R-%3D5%2BT9w192rf5iw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...