Thursday, December 3, 2020

Re: [MW:31806] Repair WPs

see the group no, no sfano. SFA no is not essential, only Group no or Fno as per ASME

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Dec 3, 2020 at 12:58 PM udaya bhaskar <dusroni@gmail.com> wrote:
Thank you for your advice.
But as per API1104 both F number is A5.5 . 
Table 1—Filler Metal Groups


On Thu, Dec 3, 2020 at 9:33 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
u can not use 7018 in place of 7010  because Fno is different which is an essential variable.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Dec 3, 2020 at 11:28 AM Jamie Reyes <jamiejrmachineco@gmail.com> wrote:
If no impacts are involved, then yes. If I'm understanding you correctly, that is.....

On Wed, Dec 2, 2020 at 7:30 PM udaya bhaskar <dusroni@gmail.com> wrote:
Dear Giants,

I want to know about little doubt on piping welding repair WPS.
WPS made with 6010 and 7010 electrodes for regular welding.
Now I can plan with  6010 and 7018 electrodes for Repair WPS on the same .
Material :API5L PSL2 grade P1G1
is it allowable?
please correct me.
--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM0cJ%3DZOxjEpLzSnLu-ujsbFjpP4pYz71G-D9VXHwwC6A%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUOEpNymfFOt3bU_uc%3DyiLvW8FQhoCx7wFDSCM%2BOH1pcGw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO7HONFXw1%2B0N8EhyTkL-p3Tpje-jXr6v7AHBQ88oF3ow%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RO5oEWD7_Rziv30ay2ja985A7N334%3DRO1UhMM83SmB0yA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePK5JhTa4Q10R1d_ka%2BQAqxRLSErOS4bGhozzOA%3DcZ5oQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...