Dear, 

You can use E6010 & E7018 for preparation of New WPS for repair, if project specification is silent about selection of electrode.

But existing WPS shall not be used with this combination of electrodes.

Regards,
CH V RAMANA 

On Thursday, 3 December, 2020, 11:28:21 am IST, Jamie Reyes <jamiejrmachineco@gmail.com> wrote:


If no impacts are involved, then yes. If I'm understanding you correctly, that is.....

On Wed, Dec 2, 2020 at 7:30 PM udaya bhaskar <dusroni@gmail.com> wrote:
Dear Giants,

I want to know about little doubt on piping welding repair WPS.
WPS made with 6010 and 7010 electrodes for regular welding.
Now I can plan with  6010 and 7018 electrodes for Repair WPS on the same .
Material :API5L PSL2 grade P1G1
is it allowable?
please correct me.
--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM0cJ%3DZOxjEpLzSnLu-ujsbFjpP4pYz71G-D9VXHwwC6A%40mail.gmail.com.
--
Regards,
Jamie Reyes
J.R. Machine Company, Inc.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJNUtUOEpNymfFOt3bU_uc%3DyiLvW8FQhoCx7wFDSCM%2BOH1pcGw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...