Dear Mr. Selvin,
Enclosing two articles towards,
1. Preheating LAS and
2. Relation between preheat & micro structure recently up loaded for your study.
The second article was published in the year 2019 in Springer Nature Journal and
will give you an idea towards preheat and micro-structure relation.
Trust it will help you.
regds,
C Sridhar.
-------------------------------------------------------------------------------------------------
On Friday, 28 February, 2020, 04:36:31 pm IST, selwin jebadas <selwinjebadass@gmail.com> wrote:
Experts,
-- I need some basic understanding from LAS welding.
1)Need for preheat in LAS?
2)Preheat & microstructure relation?
Many thanks,
Selwin
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJe433Md_wcr2%2BpdqyRJC94iULZomWNUZAzGHVby4HvWD_P2Dg%40mail.gmail.com.
Comments