Monday, February 24, 2020

Re: [MW:30544] copper materiel cladding

Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Thursday, February 20, 2020, 08:30:36 PM GMT+7, Rahul Rathod <welder.tigarc6g@gmail.com> wrote:


Dear all,

we have received a query for cladding on copper material through GMAW process, can any one suggest which welding consumables is good for cladding on copper, 
application is forging furnace cooling system, temperature is 800° to 900°degree Celsius, 
copper job thickness 20 mm 
length 450 mm round shape 
we need 3 mm build up please suggest best welding consumables for heat resistance and metal to metal wear resistance 

everyone thanks in advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6e9bd380-8e12-40d2-98c7-23c53daa2ace%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...