Re: [MW:30536] Base Metal Hardness after PWHT

Please specify the Method of measurement and instruments used ?

On Fri, Feb 21, 2020 at 12:18 PM <patelroshankk@gmail.com> wrote:
Dear Experts,

For SA 182 F11 and SA 182 F22 materials after welding and PWHT hardness of Base Metal is reduced to 120 HB, is it acceptable or not ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/abc35094-fc8b-4ed9-93a7-69bcac2d1b1c%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UPT5tvTKraGqApbVWu2M_H1kjKau8%2B7e4a9X3%3D58wZVUQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...