[MW:30510] CRO & HARDFACING QUALIFICATION

Dear Experts,

Please explain

QW-381.1

When specified as essential variables, the limitations of position and diameter qualified for groove welds shall apply to overlays welds, except the limitation on diameter qualified shall apply only to welds deposited in the circumferential direction.

How can I overlay on pipe ID & OD after qualifying welder on a plate ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP4kguv7b4EJbG2fGykaOEQRGYybBktOB%3DSrJKuwh7G3OGORLw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...