Re: [MW:30523] CRO & HARDFACING QUALIFICATION

No. For Overlay welding on pipes you should qualify with pipe only. (weld to be done in circumferential direction)

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282

E-mail : karthik6684@yahoo.com



On Wednesday, February 19, 2020, 05:09:08 PM GMT+7, Imran Khan <mikhan4k@gmail.com> wrote:


Dear Experts,

How can I weld overlay on Pipe ID & OD, by qualifying welder on a plate as per below code requirements.


(c) The essential variables of QW-350 and QW-360 shall apply for welders and welding operators, respectively, except there is no limit on the maximum thickness of corrosion‐resistant overlay that may be applied in production.When specified as essential variables, the limitations of position and diameter qualified for groove welds shall apply to overlay welds, except the limitations on diameter qualified shall apply only to welds deposited in the circumferential direction.


Warm Regards 
Imran khan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1b6c091-0145-4414-969e-ef7efad4f33d%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...