Thursday, February 20, 2020

Re: [MW:30523] Re: Impact Test

To be precious

Refer  UCS 67- Highlighted line


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Thu, Feb 20, 2020 at 11:57 AM Prashant Rane <pprane.rane1@gmail.com> wrote:
Impact for Weld is not required as E 7018-1 is upto minus 45 deg c, as per Code.  Check the GTAW Filler if you are using any.  

Most important check material of flange and pipe

Regards,
Prashant

On Wed, Feb 19, 2020, 2:09 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AMkqLQr%2BV0KXTtf%3DG%2BX03SpPg8z92ePJqHXO0PJpZctg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAkMc%3D6GaD_gJ7K9S%2Bt9%3DjDqCmyyeS1s9WxRWB6%3DZ2WDf4%2B4Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcEGt1uekabGLJqxUVR_dbu6G9Dm213djBjqPiPxY_XuBg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...