Wednesday, February 19, 2020

Re: [MW:30514] CRO & HARDFACING QUALIFICATION

Dear all

There are  standards known as API 5 LD and 5 LC, you can refer these standards. The over lays are done with automated machines. Overlaying can be done both internally and externally.

Regards
N S Gurm 

On Wed 19 Feb, 2020, 3:39 PM Imran Khan, <mikhan4k@gmail.com> wrote:
Dear Experts,

How can I weld overlay on Pipe ID & OD, by qualifying welder on a plate as per below code requirements.


(c) The essential variables of QW-350 and QW-360 shall apply for welders and welding operators, respectively, except there is no limit on the maximum thickness of corrosion‐resistant overlay that may be applied in production.When specified as essential variables, the limitations of position and diameter qualified for groove welds shall apply to overlay welds, except the limitations on diameter qualified shall apply only to welds deposited in the circumferential direction.


Warm Regards 
Imran khan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1b6c091-0145-4414-969e-ef7efad4f33d%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADHDBcDxXoBJaZJRX4QTkZZeo0L1pyMFHpv3Mrh4nn5jkAdC2g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...