RE: [SOCIAL NETWORK] [MW:30470] Miter groove weld (ASME B31 3-2018)

It is your normal butt weld and the miter is a curved portion of a pipe .

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Anna
Sent: 11 February 2020 14:39
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [SOCIAL NETWORK] [MW:30468] Miter groove weld (ASME B31 3-2018)

 

Dear All,

 

I am a translator of the construction company based in Russia. While studying ASME B31 3-2018 I faced a miter groove weld and don't quite understand what kind of weld it is and how it looks.

 

Could anyone please help me?

 

Thank you in advance.

 

Best regards, 

Anna 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/81ce42de-54d3-4531-9146-7c8e9a740658%40googlegroups.com.

---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately. Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences. While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail. ---------------------------------------------------------------------------------------------------------

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...